White Petroleum Jelly MERKUR 500 | ||
|   | Test Method | Results |
|---|---|---|
| Congealing point deg C | ASTM D.938 deg C | 49 - 52 |
| Cone penetration at 25°C | ASTM D.937 1/10mm | 140 - 160 |
| Viscosity at 100°C | ASTM D.445 mm 2/S | 5 |
| Colour lovibond 2" cell | IP 17 | 1.5 Y |
| Density at 80°C Kg ms | ASTM D.1298 | 800 |